Map showing distribution of test pits, copper assays, and pyrite footprint. Many of the test pits were completed within the strongly leached horizon and didn’t reach less oxidized material. Image from trench 26SRT-076 illustrates this oxide to sulphide transition. Hand sample from trench 26SRT-106 shows covellite coatings on fracture surfaces.