Figure 1.

The effect of roasting on the recovery of REE from the allanite feed sample

The effect of roasting on the recovery of REE from the allanite feed sample. The allanite feed sample was roasted in a muffle furnace for two hours. Leaching conditions: 1 M H2SO4, d80 = 47.9 µm, 75 ˚C, S/L ratio = 25 g/L, and 2 h.