Figure 12: SFDH-30 and 31 cross section.

Figure 12: SFDH-30 and 31 cross section.

Previous drilling by the Company at SFdLA positioned drill rigs outside the breccia, using inclined holes to test across the pipe. This drill hole geometry left the top 20-30m of the breccia pipe (the ‘oxide’ zone) under-represented. Drill holes SFDH-030 and SFDH-031 tested this oxide zone in the western half of the breccia, returning high gold grades from surface.