NAED Helium F2: From Polysilicon to Wafer
Inside the Helium F2 continuous-Czochralski furnace, a monocrystalline silicon ingot is drawn slowly from molten silicon held just above 1,414 °C in a quartz crucible. Granular silicon feeds the melt as the crystal grows, so up to five 4,000 mm ingots come from a single crucible. Right, top to bottom: polysilicon feedstock, the crucible charge, finished ingots, and wafers ready for cell production.
Format
JPEG
Source
NAED Energy Holding Inc