Figure 7

Figure 7

High-grade oxide gold mineralisation at SFdLA: Tourmaline-sericite altered siltstone clasts supported in a weathered and gossanous goethite-hematite matrix (after chalcopyrite-tourmaline). SFDH-034, 27.4m. From a 1m sample that averaged 59.1 g/t gold, 295 g/t silver and 0.07 % copper. Photograph is of a selected interval and is not necessarily representative of mineralisation hosted throughout the property.